Bob Willis

Gold boards are susceptible to the defect.

This month we look at solder spotting, which is often seen after first- or double-sided reflow, most commonly on gold boards. The two examples below illustrate what happens. FIGURE 1a shows two spots on a nickel/gold pad, and FIGURE 1b shows one spot on a copper OSP pad finish.

 

 

 